High resolution digital image correlation and electron backscattered diffraction data quantifies deformation on the surface of a Nickel-based superalloy with fine gamma prime precipitates. The data was collected after the material was subjected to 2% strain in tension. Allan Harte from the University of Manchester provided this dataset.
Use Cases
- Analyze local strain patterns based on high-resolution digital image correlation (HRDIC) data.
- Study crystallographic orientation changes based on electron backscattered diffraction (EBSD) data.
- Model the interaction between fine precipitates and deformation mechanisms based on the described material state.
- Validate computational materials science simulations against experimental deformation data.
Strengths
- Data is derived from high-resolution imaging techniques (HRDIC and EBSD).
- Focuses on a specific, well-defined material state: Nickel superalloy with 70 nm diameter precipitates after 2% tensile strain.
Limitations
- Column-level documentation is absent; field semantics must be inferred after download.
- Row count and file size are unknown, which may limit suitability assessment.
- Last update date is unknown; freshness unverified.
Provenance
- Source
- University of Manchester
- Collection Method
- Experimental data collected via High Resolution Digital Image Correlation (HRDIC) and Electron Backscattered Diffraction (EBSD).
- Time Range
- null
- Freshness
- null
- Geography
- null